Solutions for Strex Cell Stretch Systems
Autoclaving does not affect adhesion, however you should not use aluminum foil. Use special sterilized bags.
Thu, 19 Dec, 2019 at 10:41 AM
The stretch chambers made by Strex are intended for one-time use. Cross-contamination between experiments cannot be completely removed, and reuse of stretch...
Thu, 19 Dec, 2019 at 10:41 AM
The material of our stretch chambers made by Strex is a thin silicone elastomer whose main part is made of Polydimethylsiloxane (PDMS). The surface has str...
Thu, 19 Dec, 2019 at 10:41 AM
Our unique stretching system enables uniform stress loading due to the materials and methods employed and the shapes of stretch chambers. The STREX Cell Str...
Thu, 19 Dec, 2019 at 10:41 AM
The signal transduction systems and biochemical responses stimulated in the cells under sustained cellular stretching and those under periodic cellular stre...
Thu, 19 Dec, 2019 at 10:41 AM
Stretch Chambers made by Strex are non-sterile. The chamber must be autoclaved for 20 minutes at 180°C. Aluminum foil should not be used in the autoclaving ...
Thu, 19 Dec, 2019 at 10:41 AM
Yes, we can manufacture stretch chambers for mass cultures by special order.
Thu, 19 Dec, 2019 at 10:41 AM
We recommend coating the chambers just before use.
Thu, 19 Dec, 2019 at 10:41 AM
PDMS or polymerization initiators with low molecular weight may emerge, however we have never received a report saying these substances do harm on the exper...
Thu, 19 Dec, 2019 at 10:41 AM
Due to the thinness of the elastic silicone membrane, the chamber may slack in the center. The ultra-thin film (100 – 200 μm) facilitates observation of sam...
Thu, 19 Dec, 2019 at 10:41 AM